The low temperature degradation, LTD or aging, is defined as spontaneous tetragonal-to-monoclinic transformation occurring over time at low temperatures. The degradation represents thermodynamic stability, and lower transformation means less microcrack occurrence and decrease in strength.
While 21% of the tetragonal phase transformed to monoclinic for General Zirconia Disc after aging for 5 h at 132℃ and 0.2 MPa, ISO13356 standard, no degradation occurred on Perfit FS under identical conditions.



![[VATECH] Perfit FS Zirconia Block](https://apexontech.com/wp-content/uploads/2025/08/Jet-Stream-Replacement-Filter-Bags-Parts-8.png)
![[VATECH] Perfit ZR WHITE (HT/ST/UT)](https://apexontech.com/wp-content/uploads/2025/08/Jet-Stream-Replacement-Filter-Bags-Parts-12-400x400.png)
![[VATECH] Perfit ZR MULTI-LAYERS (TSML/STML)](https://apexontech.com/wp-content/uploads/2025/08/Jet-Stream-Replacement-Filter-Bags-Parts-11-400x400.png)
![[VATECH] Perfit CL Effect liquid 20ML](https://apexontech.com/wp-content/uploads/2025/08/Jet-Stream-Replacement-Filter-Bags-Parts-9-400x400.png)
![[VATECH] Perfit M 50PRO](https://apexontech.com/wp-content/uploads/2026/02/VATECH-3-400x400.png)
![[VATECH] EzCam](https://apexontech.com/wp-content/uploads/2026/02/VATECH-4-400x400.png)
![[VATECH] Perfit M 40CS](https://apexontech.com/wp-content/uploads/2026/02/VATECH-2-400x400.png)
Reviews
There are no reviews yet.